190 MICHELIN Motorcycle Scooter Tire Guide 2026 Edition
IV - THE MAIN PROBLEMS
The 7 main defects
( competition range )
crown
DESCRIPTION
Uneven wear Type of wear on crown
sawtooth wear in the rolling direction
max min wear evidence of wear
on the shoulder rail type wear
DEVELOPMENT
If wear is too pronounced risk of damage
to the crown plies
CHECKS ADVICE
Go over the history of the tire mileage
dates changed load front rear f itment etc
Check conditions of use
Check if the size is suitable and the one
recommended by the manufacturer
Check inf lation pressure
Check the mechanical condition of
suspension steering and wheel bearing
elements
Correct all mechanical anomalies
on the vehicle
Do not exceed the recommended load
DESCRIPTION
Formation of deep wrinkles ,
visible on the internal or
external shoulder of the tire .
CAUSES
The mixture is not warmed
up , the tire is outside its
window
of use .
The mixture temperature is
too low ; grip is therefore not
generated .
CHECKS / ADVICE
1 . Increase the pressure
( 1 . 8 bar maximum for the
rear ; 2 . 5 bar for the front ) .
2 . Choose a softer compound
and adapt pressure to type
of use .
3 . Adjust the bike settings
to make the rear tire work
correctly .
Inner liner
THE TIRE MUST NOT SHOW
ANY SIGNS OF MARBLING
BEFORE REPAIR .
DESCRIPTION
The marble is a pleating of
the inner liner . In the marbled
areas , the rubber is blackened
on a width which can have
dif ferent sizes .
CAUSES
Puncture , pressure loss ,
under pressure riding ,
excessive load evolutions .
DEVELOPMENT
Run - f lat riding ,
tire dislocation .
CHECKS / ADVICE
Damage can not be seen
from the outside of the tire ,
in the case of puncture , the
tire must be demounted to be
checked internally . A tire with
marbling evident is no longer
f it for continued use and
should be scrapped .
Type of wear
Graining
Tire damage / Wear
marble
TECHNICAL DATA I THE MAIN PROBLEMS